| Item | Specification |
|---|---|
| Main Composition | Yttria-stabilized Zirconia ≥94.5% |
| Density | ≥6.0 g/cm³ |
| Vickers Hardness | 1200–1350 HV |
| Sphericity | ≥0.95 |
| Wear Loss | ≤0.15 ppm/h |
| Size Range | 0.1mm–20mm |
Avoids tiny impurity shedding, ensuring high-purity finished powder during processing.
Ensures even grinding movement, enabling uniform particle size distribution and thorough material homogenization.
Prevents bead cracking and powder mixing during long-term fine milling, greatly improving production stability and product qualification rate.
Designed for fine particle production and homogenization, the beads perfectly support ultra-fine grinding, particle dispersion and batch homogenization, suitable for all types of sand mills and ball mills for high-precision fine material processing.